Mullen SD-10 PRE-RP... weird corrosion... anybody seen this?

Instruments, mechanical issues, copedents, techniques, etc.

Moderator: Dave Mudgett

User avatar
Mickey Adams
Posts: 5144
Joined: 26 Jan 2004 1:01 am
Location: Bandera Texas
Contact:

Post by Mickey Adams »

oxidation
ARTIST RELATIONS: MSA GUITARS
2017 MSA LEGEND XL D10, S10, Studio Pro S12 EXE9
Mullen G2, Rittenberry S10, Infinity D10, Zumsteel 8+9
Anderson, Buscarino, Fender, Roman Guitars, Sarno Octal, Revelation Preamps, BJS BARS, Lots of Blackface Fenders!
User avatar
Jon Snyder
Posts: 41
Joined: 8 Nov 2021 12:43 pm
Location: Nevada, USA

Post by Jon Snyder »

The aircraft industry has a treatment for this. Something about the surface prep and restoration of aluminum. Aircraft Spruce is where I have purchased the treatment in the past. Any plane that has see a lot of duty near an ocean is suspect from the salt. Might have a use here.